Thursday, 11 April 2013

Ash glaze test results

Opened the electric kiln this morning and was pleasantly surprised by the "Ki-Seto" glaze tests I did. They all came out quite dark and not terribly yellow, but I can see potential in all of them. First up is the fake ash glaze plus yellow iron oxide on the left:


I expected this would be runny, so it was placed on a broken bit of kiln shelf..and run it did! Less iron oxide next time may reduce the fluidity of the glaze a little. The Leach Old Seto Yellow (on the right above) came out very nicely, if a little thin in places. The glaze ran but stayed on the edge of the foot, luckily. Here is the test piece with Old Seto but only half the amount of ash: 


Still fairly runny, this glaze produces some yellowish hues where thicker..as well as patches of translucent, amber-coloured glaze.

Finally the Nami-Jiro glaze with additions of yellow iron oxide: 


I like the rich, matte yellow hues produced on these pieces where the glaze is thicker, but overall, the brown tones are not very exciting. The problem with many of these heavily ashed glazes is making the slop thick enough, and then preventing the glaze from deflocculating. (Update: having read a piece about Hamada's glazing technique, I've realised that for this type of ash glaze, I need to bisque much lower, perhaps only 800 - 900 degrees C. That should allow the clay to take a thicker coating of glaze, but of course one then needs to consider how to deal with bigger potential glaze runs..)

This last piece was coated with a matte ochre-ash glaze I've used many times. It also produces lovely yellow tones where thicker, but this glaze slop was made with mainly pine wood ash, so it turns a kind of blue-green  when applied very thick. The shiny patches are splashes of Oribe, turned amber by the iron in the ochre ash glaze: 


Torn vase, approx. 5 inches tall


Sunday, 7 April 2013

New clay, slips and glazes

I'm going through another experimental phase, trying out some new things and refinements of old things. First is a new clay from Potclays (new to me that is) called pink, grogged stoneware. I'm hoping this high-iron clay will be able to withstand wood firing and give interesting results under a white slip, and possibly under shinos. This tea bowl was been made with it, and I also tried out a different way of carving the footring, using a loop tool:


In my continuing search for the perfect black slip, I've also prepared a Gosu slip, based on one of the recipes in John Britt's "Complete Guide to High Fire Glazes". It's made with manganese dioxide, red iron oxide and cobalt oxide plus a little red clay. In John's book it says that the Japanese often mix their Gosu slip with a little green tea to aid application, so in the absence of green tea I tried it first with stewed, British tea. And I must say, brushwork with this mixture is a doddle due to the fine particle sizes..so smooth it's wonderful, with nice sharp, dense lines. This slip is designed to produce a greyish colour (hence "gosu", meaning mouse in Japanese) under a thin layer of shino, and is most likely unsuitable for use under a transparent glaze with such high oxide content.

Another current area of interest is Japanese, Ki-Seto glaze, a kind of satin-matte, yellow glaze containing wood ash and iron oxide (this page from e-Yakimono provides a summary of Ki-Seto terms) . So far, I've been unable to find a definitive Japanese recipe for this glaze, or establish whether one exists..many of the Ki-Seto pieces I've looked at online seem to vary alot in terms of the yellow colour, and the texture and transparency of the glaze. There is this well-known recipe called Old Seto Yellow (from Bernard Leach, I believe) which may be an approximation of the traditional Ki-Seto:

cone 8-10 /Leach:

Feldspar 25
Medium ash 50
Ochre 25


I will try the above recipe, although I suspect the material I have here is a pure yellow iron oxide, much stronger than yellow ochre which is normally an earth pigment with a high clay content. In fact I just read another blog where a potter said they tested the Leach glaze and it came out matte purple, which I think  may have been caused by an excess of yellow iron oxide. 

My version will probably look something like this: 

Potash feldspar 25
Oak wood ash 50  (I will also do a test with 25 of wood ash for comparison)
Kaolin 25
Yellow iron oxide 5

I'm modifying a Nami-jiro recipe and a fake ash glaze as well, to see if I can create an acceptable, similar version rather than an exact copy of Ki-Seto. But if anyone happens to know exactly how Japanese potters prepare it, and you'd like to share your knowledge, I'd love to hear from you!

Glaze test pieces

Above photo:  left is fake ash glaze with y.i.o., middle two are Nami-jiro with y.i.o., right is Leach Old Seto, altered as above. These will be fired to cone 10 in oxidation.









Saturday, 23 March 2013

Latest electric firing 21/03/213

A few photos of pieces from Thursday's electric firing:

Jar or vase, approx 5 inches tall

Jar or vase (b)

Water dropper, approx 2.5 inches tall

Vase, approx 4 inches tall

Lidded container, approx 3 inches tall

Guinomi, approx 3 inches tall

Carved vase, approx 3.5 inches tall

Jar or vase, approx. 3 inches tall

Bottle vase, approx 4 inches tall

Cup, approx. 2.5 inches tall
Dancing vase, approx 3.5 inches tall
Dancing vase (b)

The vase in the last photo was fired three times, first in a wood kiln, then in the electric to cone 10. I wasn't completely satisfied with it, so I dipped the top third in my new oribe glaze and fired it again to cone 10. I like this piece much more now, and was surprised how well the glaze turned out, considering it was applied to stoneware!

Wednesday, 20 March 2013

Teacaddy decoration

I decorated a teacaddy this afternoon, kind of a spur-of-the-moment decision..sometimes the best things happen when you do something spontaneous. The brushwork is black slip over an orange background, I can't wait to see how this fires.

The handle was made from the pad of clay left after wiring off a piece form the wheel..simply scraped off and scrunched into a loop.




Monday, 18 March 2013

Making handles under the warm sun

The weather is up, down and all over the place at the moment. It was pouring down on Saturday, snowing on Sunday and first thing today, beautiful spring sunshine..now it looks like it might snow again!

I spent this morning trimming cups and putting some handles on espresso cups..very enjoyable it was too, with the Beatles on the radio and the sun streaming in through the window.

Here's an example with a new handle design I've not tried before. Is the handle too big for the cup? I'm not sure yet, I'll wait and see how it looks and feels after the glaze firing.


Wednesday, 6 March 2013

Spring is here .. almost.

The days are starting to feel distinctly warmer though the mornings are still uncomfortable..and the water coming out of the workshop tap is hand-numbingly freezing! So it's onwards and upwards, time to "gain momentum" as someone said on facebook.




11th March update: I spoke to soon, it's suddenly turned arctic with temperatures around 0 degrees, and the snow has returned yet again! It's been another hard winter for making pottery.






Friday, 22 February 2013

Black iron slip test result.

As planned, I electric-fired several different slips under two types of glaze to compare the results. Both the iron slips were a 50/50 mix of the oxide and a white slip. The black magnetite slip does indeed give off oxygen at cone 10 (in oxidation), perhaps slightly more than the red iron oxide! It certainly produces different kinds of bubbles in the shino..more of a honeycomb than open pinholes. The key difference is that the black magnetite slip stays a much darker shade of brown, and looks blacker under the shino glaze (top half ).


The black iron produces a very rich, dark brown under a transparent ash glaze (bottom half)

The red iron oxide (synthetic) produced a less dark brown, which looks reddish purple under the shino. The bubbles in the glaze seem to be smaller, although this is also affected by glaze thickness. It's worth noting that where the glaze is very thick near the top of the jar, there's rather alot of pin-holing going on over the bare clay too.


Interesting that the Masons black stain has come out a very similar shade of brown to the red iron oxide under the transparent glaze, but looks darker under the shino, very similar to the magnetite slip:

slip with 20% Masons black stain
The Masons stain has also bubbled a fair bit, though less than the magnetite. To my eye, an equal mix of black and red iron slips looks more like the red iron than the black:


Finally a couple of pieces I decorated using black and red slips:

Wine cup (magnetite slip outside, red iron oxide slip inside)

Sake cup (magnetite slip)
So what have I learned from all this? Magnetite slip seems to give a richer, darker colour under transparent ash glaze, but is harder to decorate with due to the larger particle size. To minimise bubbling and pinholing with either material under shino, the secret is very thin glaze application. (I'm also wondering if a heavily crawled shino may help in allowing trapped gases to escape around the glaze) Of course I've yet to try genuine black iron oxide, FeO .. but I don't know where I can buy it. Does anyone know of a good source in the UK?